There you go. Make your own Everdur.
Yes, I was going to say the same as Petee716. I have both FeSi and Pure Silicon. But, I'm saving the pure Silicon for Bronze.
I have some extra Manganese Flake for Everdur Bronze, if anyone needs some. I can send you about 1.25 pounds for $12 includes shipping, within the...
W3 is owner of Foundreaming, which has become a meeting place for a small group of old* metal casters who became friends on Alloy Avenue. HEY! I...
Welcome, I'm up by Mansfield, Ohio. Not sure how many active Ohioans there are, actually I haven't been able to cast anything other than Pewter...
I have one I bought on ebay. It does OK for Cas Iron but it kind of subjective to where the operator decides is the vanishing point of the...
Looks like that one came out better. When I tilt the flask, I have it tilted the other way, so the metal flows up into the mold evenly.
Probably persistence, and many failures to get one good one. Like most of my foundry work. o_O
The Phos is an Iron-Phos alloy. The FeP I have is 26% Phos and the remainder is Iron. I have read that the optimum amount of Phos for thin...
I would love to have them but the shipping from Canada would be ridiculous. I would have some alloys to trade if you needed any, Manganese,...
We had a sample furnace at work that used a copper crucible, Argon gas and a tungsten electrode. I think the base was a 400 amp Miller welder. We...
Or Deadhead
Is that the travelling belt buckle pattern from AA? One was making the rounds back about 2010 I think. I don't remember who started it, maybe it...
https://youtube.com/shorts/UUz8lrxLMuI?si=e6hrhvL5sEYArVHk Check this guy's "furnace". This would be the low end furnace. Or, you can go all the...